In a BLDC or PMSM motor, the magnet is the most costly and most fragile part. The right magnet grade decides whether the motor survives heat; the right assembly process decides whether the magnets stay on the rotor at full speed.
1. Introduction
Magnet failures are usually not "bad magnets". They come from a wrong grade for the temperature, poor surface cleaning before gluing, magnets cracking from thermal expansion, or a rotor that was never designed for its top speed. This blog covers rotor types, magnet materials, grade codes and a step-by-step assembly process.
2. SPM vs IPM rotor
| Point | Surface PM (SPM) | Interior PM (IPM) |
|---|---|---|
| Magnet position | Glued on the rotor surface | Inserted into slots punched in rotor laminations |
| Torque | Magnet torque only | Magnet torque + reluctance torque |
| High-speed strength | Needs a sleeve, banding or can to hold magnets | Steel bridges hold the magnets; good for high speed |
| Field weakening (wide speed range) | Limited | Good – used in EV traction motors |
| Manufacturing | Simple, but gluing accuracy decides runout | Magnet insertion + fixing (glue/resin) into slots |
| Typical use | Fans, servo motors, small BLDC, outer-rotor hub motors | EV motors, compressors, high-efficiency industrial PMSM |
3. Magnet materials
| Material | Typical remanence Br | Max working temp (typical) | Cost | Where used |
|---|---|---|---|---|
| Ferrite (ceramic) | about 0.4 T | up to about 250 °C | Lowest | Ceiling fans, pumps, appliances |
| Bonded NdFeB | about 0.6–0.7 T | about 120–150 °C | Medium | Small BLDC, ring magnets |
| Sintered NdFeB | about 1.2–1.45 T | 80–230 °C by grade | High | EV, drones, servo, compressors |
| SmCo | about 1.0–1.15 T | about 300 °C or more | Highest | Aerospace, defence, very hot motors |
4. Reading an NdFeB grade code (example N42SH)
- N = sintered NdFeB.
- 42 = maximum energy product (BH)max in MGOe – higher number, stronger magnet.
- SH = coercivity / temperature class. Suffix ladder (approx. max working temperature): none 80 °C → M 100 °C → H 120 °C → SH 150 °C → UH 180 °C → EH 200 °C → AH 230 °C.
- N42 has Hcj above 12 kOe and works to about 80 °C; N42SH has Hcj above 20 kOe and works to about 150 °C.
- Br drops about 0.11–0.12 % per °C, and coercivity drops about 0.4–0.7 % per °C. Hot magnets are weaker and easier to demagnetise.
- Higher temperature classes use dysprosium/terbium, so they cost more and have slightly lower Br.
Maximum working temperature also depends on magnet shape and the motor's magnetic circuit; always check the demagnetisation curve at your hottest operating point and peak current.
5. Magnet assembly process – step by step
- Incoming check: dimensions, coating (NiCuNi or epoxy), grade marking, flux of sample pieces.
- Surface preparation: degrease rotor and magnet surfaces; light abrasion or primer where the adhesive maker specifies.
- Adhesive dispensing: controlled bead or film; glass-bead spacers or film adhesive keep a thin, even bond line.
- Magnet placement or insertion: fixture holds each magnet at exact angle (SPM), or magnets are pushed into lamination slots (IPM) by machine.
- Cure: time and temperature as per adhesive datasheet, rotor held in fixture.
- Retention (SPM, high speed): glass/carbon-fibre banding, stainless can or sleeve against centrifugal force.
- Balancing: dynamic balancing of the full rotor.
- Magnetising: often done after assembly with a multipole magnetising fixture – safer handling and exact pole pattern.
- Final check: flux/pole pattern scan, runout, back-EMF test after motor assembly.
6. Common problems – root cause – solution
| Problem | Root cause | Solution |
|---|---|---|
| Magnet comes loose at high speed | Poor surface cleaning; adhesive not cured; no retention sleeve | Fix surface prep and cure control; add banding/can; design rotor for overspeed |
| Cracked magnets | Thermal expansion mismatch between magnet and rotor; impact during handling | Flexible-tough adhesive and thin bond line; handling fixtures; avoid magnet-to-magnet impact |
| Motor loses power after hot running | Grade too low for temperature; high demagnetising current | Move up the suffix ladder (H → SH → UH); limit peak current; improve cooling |
| Vibration and noise | Magnet position error, uneven bond line, rotor imbalance | Precise fixtures, controlled bond line, dynamic balance |
| Hot magnets in high-speed motor | Eddy currents inside solid magnets | Segment (laminate) magnets axially and circumferentially |
| Rust on magnets | Coating damaged | Specify coating for environment; protect during assembly |
Safety note: large NdFeB magnets snap together with great force and can crush fingers. Use non-magnetic tools and fixtures.
7. Videos to watch (18)
| # | Video | Channel | Length | Why watch |
|---|---|---|---|---|
| 1 | A Brief Explanation of Permanent Magnet AC Motors | ElectrArc240 | 4:47 | Quick PM motor basics |
| 2 | Module 29: Permanent Magnet Rotor Design (SPM & IPM) | CUSP | 38:50 | Design lecture on both rotor types |
| 3 | PM Machine Design – Interior Permanent Magnet (IPM) | Rotor Dynamics 101 | 6:04 | IPM rotor explained |
| 4 | EV Motor Mania: Induction vs Permanent Magnet | Munro Live | 29:18 | Teardown view of real EV rotors |
| 5 | How the World's Strongest Magnets Are Made (Neodymium) | Worldnite Journey | 8:42 | Magnet production |
| 6 | Manufacturing Processes for Sintered NdFeB Magnets | X-Mag | 2:43 | Short process overview |
| 7 | Rare Earth Magnets – How They're Made | MP Materials | 4:39 | From rare-earth ore to magnet |
| 8 | Magnets – How It's Made | Discovery UK | 5:09 | Classic factory documentary |
| 9 | Automatic Magnet Insertion Machine for BLDC Rotor | NIDE Group | 1:29 | Automated magnet insertion |
| 10 | Rotor Processing – Insert Magnet (EV Rotors) | Una Zhang | 0:34 | IPM magnet insertion |
| 11 | Magnet Gluing for EV Rotor | AMT | 1:18 | Automated gluing |
| 12 | Magnet Bonding for Electric Motors (Dispensing) | bdtronic GmbH | 1:42 | Adhesive dispensing process |
| 13 | How to Insert Magnets into a Wheel Hub Motor | NIDE Group | 1:49 | Outer-rotor magnet fitting |
| 14 | How to Put Magnets on a BLDC Rotor | George Chaniotakis | 5:18 | Hands-on SPM magnet fitting |
| 15 | Magnetising Technology – Dr Chris Riley | e-Magnets | 38:20 | How magnetisers and fixtures work |
| 16 | Industrial Magnetiser for the Automotive Sector | e-Magnets | 2:02 | Rotor magnetising in production |
| 17 | How to Reduce Eddy Current Loss in Motor Magnets (Segmented Magnets) | HQ Magnet | 5:56 | Why magnets are segmented |
| 18 | Introduction to Torque Ripple and Cogging Torque | HBK Electric Power Testing | 7:32 | How magnet design affects smoothness |
8. Sources referred
- Sintered NdFeB Magnet Grades – N42 vs N42SH, Advanced Magnets
- Neodymium Magnet Grades Chart – Radial Magnet (suffix ladder, Dy/Tb trade-off)
- Neodymium Iron Boron Magnet Catalog – Arnold Magnetic Technologies (N42SH data, temperature coefficients)
- Complete Guide to High-Temperature Neodymium Magnets – Stanford Magnets (coercivity temperature coefficient)
- US Patent 9130426 – Permanent magnet rotors and methods of assembling (adhesive bonding failures)
- US Patent 9819236 – Coupling permanent magnets to a rotor body (thermal expansion cracking)
- Epoxy Adhesive for Bonding Magnets in Motors – Incure (surface prep, bond line control)
Share your experience. Have winding data, a shop-floor photo or a doubt on this topic? Join the MotorMakers India community and help others learn.